Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy EXGY30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy FXTW30PE ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Geloy FXTW30CP ASA
Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -30.0 - 30.0 °C
60.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10
LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 40.0 °C
60.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS
LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -30.0 - 30.0 °C
60.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON SD000 PA12
LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT (Europe-Africa-Middle East)
LNP* THERMOCOMP* WF006 is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 37.8 °C
60.0 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade
Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a..
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature -40.0 - 37.8 °C
60.0 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Diamond Polymers DIAMALOY GLY 9020 Sheet Extrusion Grade
Diamaloy GLY 9020 resin is a high-gloss, low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, an..
CTE, linear, Transverse to Flow 108 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding
Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar.