Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 11.9 µm/m-°C @Temperature 20.0 °C |
6.61 µin/in-°F @Temperature 68.0 °F |
Crosswise; ASTM D696 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |