Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP COLORCOMP J1000 PES (Europe-Africa-Middle East)
LNP* COLORCOMP* J1000 is a compound based on Polyethersulfone resin.
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 20.0 °C
32.8 µin/in-°F

@Temperature 68.0 °F
Eastman Eastapak 9921W PET  (discontinued **)
Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 20.0 °C
32.8 µin/in-°F

@Temperature 68.0 °F
Eastman Eastar GN101 PETG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 0.000 - 100 °C
32.8 µin/in-°F

@Temperature 32.0 - 212 °F
ASTM E381
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded  
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre..
CTE, linear, Transverse to Flow 59.0 - 78.1 µm/m-°C
32.8 - 43.4 µin/in-°F
Average value: 67.6 µm/m-°C Grade Count:15
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East)
LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU (Europe-Africa-Middle East)
LNP* THERMOCOMP* GF006 is a compound based on Polysulfone resin containing Glass Fiber.
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber.
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
32.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized .
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
32.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT
LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage.
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
32.8 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
CTE, linear, Transverse to Flow 59.0 µm/m-°C
32.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
32.8 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve..
CTE, linear, Transverse to Flow 59.0 µm/m-°C
32.8 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 59.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
32.8 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..
CTE, linear, Transverse to Flow 59.0 µm/m-°C
32.8 µin/in-°F
z, before Tg; IPC TM-650 2.4.24
Arlon 25FR Low-Cost Ceramic Hydrocarbon
High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont..
CTE, linear, Transverse to Flow 59.0 µm/m-°C
32.8 µin/in-°F
TMA
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound
Medium flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited f..