Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 55.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP PDX-U-05314 PPA (Asia Pacific) LNP* Lubricomp* PDX-U-05314 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 55.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS PPE+PS blend. High Heat. Translucent with yellow tint in natural color. FDA compliant. Extrusion and Injection Molding. Typical applications include High Performance Food Packaging, Electronics and .. |
|||
CTE, linear, Transverse to Flow | 55.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Extrusion. Microwavable. Food, electrical/electronic packaging uses. |
|||
CTE, linear, Transverse to Flow | 55.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PN275 PPE+PS PPE+PS with low mineral loading. High heat, platable applications. |
|||
CTE, linear, Transverse to Flow | 55.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PN275F PPE+PS PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications. |