Polymer Property : CTE, linear, Transverse to Flow = 55.1 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 99.1 - 99.1 µm/m-°C

@Temperature 26.0 - 200 °C
55.1 - 55.1 µin/in-°F

@Temperature 78.8 - 392 °F
Average value: 99.1 µm/m-°C Grade Count:1
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..