Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 48.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 1285 PEI
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.
CTE, linear, Transverse to Flow 48.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 1285 PEI (Asia Pacific)
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors.
CTE, linear, Transverse to Flow 48.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics ULTEM DU319 PEI
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.