Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 78.5 µm/m-°C @Temperature -30.0 - 30.0 °C |
43.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66 LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized. |
|||
CTE, linear, Transverse to Flow | 78.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF VFK33S PA 66 LNP THERMOTUF* VFK33S is a compound based on Nylon resin containing Glass Fiber, Mineral. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 78.5 µm/m-°C @Temperature 26.0 - 200 °C |
43.6 µin/in-°F @Temperature 78.8 - 392 °F |
ASTM D696 |
Saint-Gobain Fluoroloy® A22 High Performance Seal Material High modulus with excellent high-temperature resistance; Abrasion resistant; Chemically Inert; Recommended for back-up rings and for special applications.
Information provided by Saint-Gobain P.. |