Polymer Property : CTE, linear, Transverse to Flow = 41.4 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 74.6 µm/m-°C

@Temperature 23.0 - 80.0 °C
41.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXD101R PC (Europe-Africa-Middle East)
Transparent/translucent PC for light diffusion special effects. Thicker sections without sinks. Internal mold release. Pigment package may affect properties. Application testing always recommended..
CTE, linear, Transverse to Flow 74.6 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC
LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing.
CTE, linear, Transverse to Flow 74.6 µm/m-°C

@Temperature 23.0 - 80.0 °C
41.4 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXG101 PC (Europe-Africa-Middle East)
FXG101 is a Lexan PC Translucent Grade in our VisualFX Portfolio. The Grade was developed to meet the Aesthetic Differentiation requirements of today´s Customers. Color package may effect prope..