Polymer Property : CTE, linear, Transverse to Flow = 40.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 73.2 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXE163R PC (Europe-Africa-Middle East)
LEXAN FXE163R is a transparent/translucent UV stabilized, medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE163R contains a relea..
CTE, linear, Transverse to Flow 73.2 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.7 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Lexan® FXM163R PC (Europe-Africa-Middle East)
PC with Visual Effect, UV-Stabilizer, Heat Stabilized, Opaque. Colour package may affect properties. Application testing always recommended.