Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 7.83 µm/m-°C

@Temperature -40.0 - 40.0 °C
4.35 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP QF00A PA6.10
LNP* THERMOCOMP* QF00A is a compound based on Nylon 6/10 containing 50% Glass Fiber.