Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 38.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
21.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s). |