Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 245 µm/m-°C
136 µin/in-°F
z, above Tg; IPC TM-650 2.4.24
Arlon 51N Lead-Free Compatible Epoxy Low-Flow
51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili..