Polymer Property : CTE, linear, Transverse to Flow = 225 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 225 µm/m-°C
125 µin/in-°F
z, above Tg; IPC TM-650 2.4.24
Arlon 45NK Woven Kevlar® Reinforced Laminate and Prepreg
45NK is a woven Kevlar® aramid fiber reinforced multifunctional epoxy laminate system engineered to provide in-plane CTE values as low as 6 ppm/°C for compatibility with leadless alumina ceramic c..