Polymer Property : CTE, linear, Transverse to Flow = 22.1 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 22.1 µm/m-°C

@Temperature -34.4 - 93.3 °C
12.3 µin/in-°F

@Temperature -30.0 - 200 °F
perpendicular to all filaments; ASTM D696-42T
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Unidirectional
CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li..