Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 31.8 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 31.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |