Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 13.7 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
7.61 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP130HF Glass Fabric
Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens..