Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 0.800 µm/m-°C @Temperature 25.0 - 1500 °C |
0.444 µin/in-°F @Temperature 77.0 - 2730 °F |
Perpendicular to pressing direction |
Momentive Performance Materials HBC Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |