Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-28EH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-28UH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-30EH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-30UH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-35 Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-35H Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-35SH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-38 Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-38SH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-40H Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-40M Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-40SH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-42 Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-42M Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-42SH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-44H Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-45 Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-45M Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-50 Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-30EZ Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-33 Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-33H Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-33SH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-33UH Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-38H Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-38M Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-40 Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-42H Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-33M Neodymium Iron Boron Magnetic Material |
|||
CTE, linear, Transverse to Flow | -1.00 µm/m-°C @Temperature 23.0 °C |
-0.556 µin/in-°F @Temperature 73.4 °F |
|
Alliance N-48 Neodymium Iron Boron Magnetic Material |