Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C

@Thickness 3.20 mm
127 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Xenoy® 6620 PBT+PC
PBT+PC, Unreinforced, impact modified thermoplastic alloy. Outstanding impact at low temperature