Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 52.0 °C @Thickness 3.20 mm |
126 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 315 PBT (Asia Pacific) General purpose polyester. Fully imported product from USA |