Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 230 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 230 °C

@Thickness 6.40 mm
446 °F

@Thickness 0.252 in
unannealed; ASTM D648
Westlake Plastics Tempalux® 5000 Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi..