Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 193 °C @Thickness 6.40 mm |
379 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Valox® 830R PBT (Asia Pacific) 30% glass filled, release grade, polyester alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |