Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C @Thickness 3.18 mm |
178 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX 92052 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.1 °C @Thickness 3.18 mm |
178 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 3.20 mm |
178 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl N190A PPE+PS (Asia Pacific) Low heat, flame retardant PPO/HIPS alloy. Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region. |