Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 6.40 mm |
176 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 6.40 mm |
176 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C @Thickness 3.20 mm |
176 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl PX6021 PPE+PS (Asia Pacific) Low heat, flame retardant PPO/HIPS alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |