Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 71.9 °C @Thickness 3.18 mm |
161 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5005 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |