Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C @Treatment Temp. 50.0 °C, Thickness 3.18 mm |
192 °F @Treatment Temp. 122 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX E1502 Polyvinyl Chloride Alloy (PVC Alloy) VSI FLAMMABILITY:Burn Length (0.040 in Bar)ASTM D635 0* IN.Burn Time (0.040 in Bar) ASTM D635 0* Sec.*Extinguished before 25 MM starting ref mark.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.9 °C @Thickness 3.18 mm |
192 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol.. |