Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 79.4 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C

@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
175 °F

@Treatment Temp. 140 °F,
Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO..
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C

@Treatment Temp. 50.0 °C,
Thickness 3.18 mm
175 °F

@Treatment Temp. 122 °F,
Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO..
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C

@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
175 °F

@Treatment Temp. 140 °F,
Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Dry Blend E7009 Polyvinyl Chloride, Rigid (PVC, Rigid)
Recommended for whites and light pastel colors only. Not to be used for darker colors.Physical properties based on Geon E7009 white 1024 lot# UTCX 57572Information provided by PolyOne