Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C @Treatment Temp. 50.0 °C, Thickness 3.18 mm |
169 °F @Treatment Temp. 122 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C @Thickness 3.18 mm |
169 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 76.1 °C @Thickness 6.35 mm |
169 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M5200 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |