Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 68.9 °C @Thickness 6.35 mm |
156 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |