Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 123 °C

@Thickness 3.20 mm
253 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.
Deflection Temperature at 0.46 MPa (66 psi) 123 °C

@Thickness 3.20 mm
253 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Asia Pacific)
PC+ABS blend, low gloss and UV-stable, suitable for automotive interior applications.