Deflection Temperature at 0.46 MPa (66 psi) 122 °C

@Thickness 3.20 mm
252 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific)
Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi..
Deflection Temperature at 0.46 MPa (66 psi) 122 °C

@Thickness 3.20 mm
252 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Deflection Temperature at 0.46 MPa (66 psi) 122 °C

@Thickness 3.20 mm
252 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
Deflection Temperature at 0.46 MPa (66 psi) 122 °C

@Thickness 3.20 mm
252 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East)
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..