Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 215 °C @Thickness 6.40 mm |
419 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific) UV-Stabilized version of 420SE0. |