Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 203 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C

@Thickness 3.18 mm
203 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ HTX Ultra LA427Plus Polyvinyl Chloride Alloy (PVC Alloy)
Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties based on Geon HTX Ultra LA427Plus Natural 0000Information provided by PolyOne
Copyright © lookpolymers.com All Rights Reserved