Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C

@Thickness 3.18 mm
195 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de..