Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 88.3 °C @Treatment Temp. 50.0 °C, Thickness 3.18 mm |
191 °F @Treatment Temp. 122 °F, Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy) Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 88.3 °C @Thickness 3.18 mm |
191 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880... |