Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C @Thickness 3.18 mm |
180 °F @Thickness 0.125 in |
Injection Molded; Annealed; ASTM D648 |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.2 °C @Thickness 6.35 mm |
180 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 82.0 °C @Thickness 3.20 mm |
180 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |