Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.9 °C

@Treatment Temp. 60.0 °C,
Thickness 3.18 mm
174 °F

@Treatment Temp. 140 °F,
Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid)
Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 78.9 °C

@Thickness 3.18 mm
174 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid)
Physical properties based on Geon L6607 white 1363Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 78.9 °C

@Thickness 3.18 mm
174 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 78.9 °C

@Thickness 3.18 mm
174 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Dry Blend E7000 Polyvinyl Chloride, Rigid (PVC, Rigid)
60 degree gloss comparisons: Geon E7000 is 47-49;Geon E7456 is 40-49;Geon E7130 is 38-43;Geon E7370 is 26-31Information provided by PolyOne