Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C @Thickness 6.35 mm |
171 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C @Thickness 6.35 mm |
171 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 77.3 °C @Thickness 3.18 mm |
171 °F @Thickness 0.125 in |
Injection Molded; Unannealed; ASTM D648 |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |