Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 124 °C @Thickness 6.40 mm |
255 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 124 °C @Thickness 3.20 mm |
255 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL REN501 PPE+PS Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only. |