Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 108 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C

@Thickness 3.20 mm
226 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PVX524 PPE
PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT