Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 96.1 °C | 205 °F | ASTM D-4065 |
CMT Materials REN Shape® 450 Prototype Tool & Modeling Board REN Shape 450 is the preferred modeling board for pattern makers throughout the world. The outstanding dimensional stability and its ability to hold precise tolerances even after exposure to heat h.. |