Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | >= 500 °C | >= 932 °F | |
UBE UPILEX 75S (75 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |
|||
Glass Transition Temp, Tg | >= 500 °C | >= 932 °F | |
UBE UPILEX 25S (25 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |