Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 87.5 °C | 190 °F | DSC |
CRP Technology Windform® PS Polystyrene for Selective Laser Sintering Windform® PS is a polystyrene based material, developed specifically to produce complex investment casting patterns. The sintered patterns are ideal for conventional wax infiltration, and become ea.. |