Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 84.0 °C | 183 °F | |
Eastman Eastar DN007 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 84.0 °C | 183 °F | DSC |
Kolon NOPLA® KE831 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Glass Transition Temp, Tg | 84.0 °C | 183 °F | |
Eastman Eastar DN003 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 84.0 °C | 183 °F | |
Epoxyset Epoxibond EB-347 Low Expansion Epoxy Adhesive EB-347 is a highly filled, low coefficient expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensiona.. |
|||
Glass Transition Temp, Tg | 84.0 °C | 183 °F | |
Armstrong A-2/E Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Glass Transition Temp, Tg | 84.0 °C | 183 °F | Cured property; Perkin Elmer TMS-2 |
Aptek 6109-A/B Epoxy Encapsulant Optoelectronic grade flexible water clear encapsulant. Higher viscosity/lower Tg version for clear blob-top encapsulation of ceramic substrate devicesPart A is blue. Part B is clear to pale yellow.I.. |