Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 368 °C | 694 °F | DMTA |
Ensinger TECASINT 1011 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |