Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 57.2 - 61.1 °C | 135 - 142 °F | Cure: 20 min./120°C; Post cure: 4 h/145°C |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |