Polymer Property : Glass Transition Temp, Tg = 5.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -7.00 - 5.00 °C
19.4 - 41.0 °F
Average value: -2.00 °C Grade Count:3
Overview of materials for Silicone Polyurethane, Polycarbonate Based
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim..