Thermal Properties Metric English Comments
Glass Transition Temp, Tg 249 °C
480 °F
ASTM D3418
DuPont Performance Polymers VESPEL TP-8311 Polyimide
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b..
Glass Transition Temp, Tg 249 °C
480 °F
ASTM D3418
DuPont Performance Polymers VESPEL TP-8541 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and impact performance in high temperature environmentsInformation provided by DuPont Performance Polymers
Glass Transition Temp, Tg 249 °C
480 °F
ASTM D3418
DuPont Performance Polymers VESPEL TP-8549 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance..
Glass Transition Temp, Tg 249 °C
480 °F
ASTM D3418
DuPont Performance Polymers VESPEL TP-8556 Polyimide
Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Perform..