Polymer Property : Glass Transition Temp, Tg = 47.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 43.0 - 47.0 °C
109 - 117 °F
ASTM E1545-00
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features..