Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 6.75 °C | 44.2 °F | Ultimate Tg |
Tra-Con Tra-Duct 2921 Silver-Filled Adhesive Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 6.75 °C | 44.2 °F | Ultimate Tg |
Tra-Con Tra-Duct 2929 Room Temperature Conductive Flexible Silver Epoxy Adhesive TRA-DUCT 2929 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy a.. |